Macquarie Semiconductor and Technology on behalf of Macquarie (Asia) Pte Ltd. Taiwan Branch - UMC

ASM International Eagle XP EmerALD

Disclaimer

The images and data contained herein is owned by Macquarie and is intended for use only by potential purchasers of goods shown herein. Except for such permitted usage, no other use of the images and data is permitted and such images and data shall not be exhibited or shown in any websites or social media or for any commercial purposes without Macquarie’s written permission. Therefore, no seller of goods like the goods shown herein has any right or authority to show or exhibit any images or data shown herein.


Asset ID: 205091

Enquire about this product Print spec sheet

ASM International

Eagle XP EmerALD

ALD (Atomic Layer Deposition)

Deposition Equipment

Equipment details:

Date of Manufacture: 2012-01-01

Currently Configured for: 300mm

Current Equipment Status: Available

Asset HDD not included

Location of Equipment: Tainan 744, Taiwan

Available date: Currently Available

HARD DRIVE WILL BE REFORMATTED. OPERATING SOFTWARE IS NOT INCLUDED.


Inspect to confirm configuration and condition.

The mainframe has been removed to other fab, so it is impossible to determine whether the remaining parts are damaged or can used adn there is only one chamber(EmerALD 3000) left on this equipment.

Configuration :

Tool Model : XP Platform

System SW(OS) version is Ver 1. 58a1-001

All cables are present

Have missing /damaged parts need inspection to confirm.

Robot Type is Yawuski

Power Supply & AC Dist Box : P/N 1060-625-01

Backing Pump(s) : ALD/LL/WHC is EDWARDS-IXH1210

Heater Jacket : INTRACO TAIWAN CORPORATION

Facility Requirements :

CDA LLC PN2 : 403

DIW : 2.95

Vacuum Load Port vacuum : -86.2

Gas LLC Pressure : 0.56/0.209 MPA

FI : 100 Pa

Ar : 500 SCCM

N2 : 500 SCCM

Ar : 3 SLM

Differential : 3.5 Pa

Product images

The information referenced on this page is accurate to the best of our knowledge. We do not warrant the completeness or accuracy of the information contained herein. Interested parties are encouraged to request inspection to verify equipment condition, configuration, and completeness. Any offer to purchase equipment shall be subject to our standard terms and conditions of sale.


Learn more -

Enquire about this product

I agree to receive further communication from Macquarie Group Limited in accordance with its Privacy Policy, as amended from time to time.

Related products

No results message:
Displayed when filters returns no results.

We couldn't find any items that match your criteria.

Please try a different keyword.

Service unavailable:
Displayed when filter service cannot be reached.

Sorry, this service is currently unavailable.

Please try again later.

Get in touch

Have a question for our team?

Ask about our equipment solutions, ranging from Macquarie equipment inventory sales, sourcing programs, surplus disposition options, and direct equipment purchases.

I agree to receive further communication from Macquarie Group Limited in accordance with its Privacy Policy, as amended from time to time.