Macquarie Semiconductor and Technology on behalf of Intel Resale Corporation
The images and data contained herein is owned by Macquarie and is intended for use only by potential purchasers of goods shown herein. Except for such permitted usage, no other use of the images and data is permitted and such images and data shall not be exhibited or shown in any websites or social media or for any commercial purposes without Macquarie’s written permission. Therefore, no seller of goods like the goods shown herein has any right or authority to show or exhibit any images or data shown herein.
Date of Manufacture:
Currently Configured for: 300mm
Current Equipment Status: Available
Asset HDD not included
Location of Equipment: Portland, United States
Available date: Currently Available
· XP8 Platform
· Front and rear Operations/Maintenance Touch Screen with pen
· Loader module transfer robot and controller with 3 load ports.
· 2 Load locks
· Wafer cooling chamber
· Four BOC Edwards dry pump (subject to availability)
· Exhausted gas box with 8 MFC capability per chamber
· 2 RF generators and controller per chamber
· Remote plasma cleaning (RPU) per chamber
· Two RF matchers per chamber
· Additional details available upon request
The information referenced on this page is accurate to the best of our knowledge. We do not warrant the completeness or accuracy of the information contained herein. Interested parties are encouraged to request inspection to verify equipment condition, configuration, and completeness. Any offer to purchase equipment shall be subject to our standard terms and conditions of sale.