Macquarie Semiconductor and Technology on behalf of Micron Memory Japan, K.K. (F15)
The images and data contained herein is owned by Macquarie and is intended for use only by potential purchasers of goods shown herein. Except for such permitted usage, no other use of the images and data is permitted and such images and data shall not be exhibited or shown in any websites or social media or for any commercial purposes without Macquarie’s written permission. Therefore, no seller of goods like the goods shown herein has any right or authority to show or exhibit any images or data shown herein.
Date of Manufacture: 2020-04-01
Currently Configured for: 300mm
Current Equipment Status: Available
Asset HDD not included
Location of Equipment: Hiroshima, Japan
Available date: 12/12/2025
Deinstallation is to be done by the OEM.
Tool config is based on original PO, please verify tool details at tool inspection
OEM: ASM
Tool Model: XP4
Chamber Name 1: Chamber 1
Chamber Name 2: Chamber 2
Chamber Name 3: Chamber 3
Chamber Name 4: Chamber 4
Chamber 1 Description: PM1
Chamber 2 Description: PM2
Chamber 3 Description: PM3
Chamber 4 Description: PM4
Chamber 1 Chemicals Gases Used: TMA, H2O
Chamber 2 Chemicals Gases Used: TMA, H2O
Chamber 3 Chemicals Gases Used: TMA, H2O
Chamber 4 Chemicals Gases Used: TMA, H2O
Damage/Missing parts list
Please inspect tool to reconfirm
Dry pumps and customer provided items not included on sales
The information referenced on this page is accurate to the best of our knowledge. We do not warrant the completeness or accuracy of the information contained herein. Interested parties are encouraged to request inspection to verify equipment condition, configuration, and completeness. Any offer to purchase equipment shall be subject to our standard terms and conditions of sale.